ALLOY:- PHOSPHORUS BRONZE (GRADE-2)
STANDARD :- IS: 28-1985
CHEMICAL COMPOSITION |
MIN (%) |
MAX(%) |
Copper (cu) |
BALANCE |
Tin (Sn) |
10.00 |
11.50 |
Lead (Pb) |
- |
0.25 |
Zinc (Zn) |
- |
0.05 |
Phosphorus (P) |
0.50 |
- |
Nickle (Ni) |
- |
0.10 |
Iron (Fe) |
- |
0.10 |
Antimony (Sb) |
- |
- |
Aluminium (Al) |
- |
0.01 |
Silicon (Si) |
- |
0.02 |
MECHANICAL PROPERTIES |
Minimum Values |
Molding Process |
Sand Casting |
Continuous Casting |
Tensile Strength Rm (MPa) |
220 |
250 |
0,2% Proof Strength Rp0,2 (MPa) |
140 |
170 |
Elongation (%) |
6 |
6 |
Hardness |
65 |
80 |
EQUIVALENT INTERNATIONAL STANDARD |
STANDARD |
ALLOY |
BS 1400 |
PB 1 |
DIN 1705 |
CuSn10 |
EN 1982 |
CuSn10- C, CB480K |
ASTM B505 |
C90700 & C92700 |
JIS H5121 |
CAC 502 C |
TECHNICAL CHARACTERISTIC |
Offers excellent mechanical strength and structural integrity. |
Suitable for high temperatures, Can handle elevated temperature applications. |
It Demonstrates resistance to corrosion in various environments, making it suitable for applications exposed to moisture or chemicals. |
Offers dependable performance and long-term durability, making it a trusted choice for critical applications in diverse industries. |